IR juriya masterbatch zafi rufi granules don taga fim samar

Heat resistant thermal rufi infrared toshe IR garkuwar infrared kin anti-infrared anti-UV masterbatch

 

 

Samfura

Babban rufin zafi na VLT Anti-IR Masterbatch

Low VLT zafi rufi Anti-IR Masterbatch

Lambar

Farashin CF-PET

(bas polymer customized)

Farashin S-PET

(bas polymer customized)

Bayyanar

Baƙar fata masu launin shuɗi

Baki barbashi

Abu mai aiki

Tungsten oxide

Tungsten vanadium tin antimony gauraye karfe oxide

Ingantacciyar abun ciki (%)

6.0± 0.2 (800 ℃, 3h)

6.0± 0.2 (800 ℃, 3h)

Fihirisar narkewa (MI, dL/g)

10.0± 2.0

10.2 ± 2.0

Dankowar ciki (IV, g/10min)

0.60± 0.05

0.58± 0.05

Matsayin narkewa (℃)

260± 10

260± 10

Danshi (%)

≤0.03

≤0.03

Haze(%)

≤1

≤1

Yawan yawa (g/cm3)

1.4

1.35

Nauyin barbashi 100(g)

1.8

1.34

Manu.Fim ko allo VLT%

≥70

≤50

--

 

-14

 

 

 

 

 

 